The plasma-resistant element is obtained by forming a liquid mixture by mixing yttrium oxide powder and nanocarbon powder having the average particle size of approximately 1 nm to 200 nm with a solvent, forming the liquid mixture into a spherical powder mixture by using a spray dryer, and by forming the sintered body from the spherical powder mixture by hot pressing.