English[en]
In addition, a fiber material for use as a cushion material is provided in the present invention, in which 80 to 60 wt% of the PCT hollow fiber having a melting point of 280 to 290̊C is combined by means of 40 to 20 wt% of a binder fiber having a low melting point as compared with the PCT hollow fiber.
French[fr]
De plus, une matière fibreuse en vue d'une utilisation comme matière de coussin est fournie dans la présente invention, dans laquelle 80 à 60 % en poids des fibres creuses de PCT ayant un point de fusion de 280 à 290°C sont combinés au moyen de 40 à 20 % en poids d'une fibre de liant ayant un point de fusion bas par comparaison avec les fibres creuses de PCT.
Korean[ko]
또한, 본 발명은 융점 280∼290°C을 가지는 PCT 중공사 80 내지 60중량%가 상기 PCT 중공사 대비 용융점이 낮은 바인더 섬유 40 내지 20중량%로 결속된 쿠션재용 섬유기재를 제공함으로써, PCT 소재의 고유물성뿐 아니라, 중공특성이 유지되어 경량성 및 쿠션기능이 최적화된다.