English[en]
For Cerrejón coal, the highest vitrinite recovery (63.55%) was obtained at pH 7, Jg 0.7 cm/s and FC of 4 ml de frother/kg of coal, whereas for Jagua coal, the highest vitrinite recovery (69.80%) was obtained at pH 4, Jg 1.4 cm/s, and 4 ml of frother/kg of coal respectively.
Spanish[es]
Para el carbón Cerrejón, la mayor recuperación de vitrinita (63.55%) se obtuvo a pH 7, Jg 0.7 cm/s and 4 ml de espumante/kg de carbón, mientras que para el carbón Jagua, la mayor recuperación de vitrinita (69.80%) se obtuvo a pH 4, Jg 1.4 cm/s and 4 ml de espumante/kg de carbón respectivamente.