[Solution] This problem is solved by using a production method provided with: a preparation step for preparing a 4-valent vanadium ion solution in which the total mass percent of one or more elements selected from aluminum, calcium, sodium, potassium, iron, silicon and chromium is less than 0.4 mass%, and dissolved oxygen is 0.1ppm or less; and an electrolysis step for obtaining a 5-valent vanadium ion solution by oxidizing and electrolyzing the 4-valent vanadium ion solution in a deaerated atmosphere, and simultaneously obtaining a divalent vanadium ion solution by reducing and electrolyzing the 4-valent vanadium ion solution in a deaerated atmosphere.
French[fr]
A cet effet, selon l'invention, on utilise un procédé de fabrication qui comporte : une étape de préparation, consistant à préparer un solution d'ions vanadium 4-valents dans laquelle le pourcentage massique total d'un ou plusieurs éléments choisis parmi l'aluminium, le calcium, le sodium, le potassium, le fer, le silicium et le chrome est inférieur à 0,4 % en masse, et l'oxygène dissous représente 0,1 ppm ou moins ; et une étape d'électrolyse, consistant à obtenir une solution d'ions vanadium 5-valents par oxydation et électrolyse de la solution d'ions vanadium 4-valents dans une atmosphère désaérée, et à obtenir simultanément une solution d'ions vanadium divalents par réduction et électrolyse de la solution d'ions vanadium 4-valents dans une atmosphère désaérée.
Japanese[ja]
4質量%未満であり、溶存酸素が0.1ppm以下の4価のバナジウムイオン溶液を準備する準備工程と、4価のバナジウムイオン溶液を脱気雰囲気で酸化電解して5価のバナジウムイオン溶液を得ると同時に、4価のバナジウムイオン溶液を脱気雰囲気で還元電解して2価のバナジウムイオン溶液を得る電解工程とを備える製造方法により、上記課題を解決する。

History

Your action: